| MATERIAL CHARACTERISTICS |
| FULLSTAR MATERIAL |
INITIAL PERMEABILITY |
PRACTIACL FREQUENCY |
RESIDUAL FLUX DENSITY(Br) |
SATURATION FLUX DENSITY(Bs) |
MAGNETIZING FORCE |
CURIE TEMP |
MATERIAL DENSITY |
(Ω-CM) |
| UNIT |
μi±25% |
MHz |
Gauss |
Gauss |
Oested |
℃ |
g/cm3 |
| D50 |
50 |
0.5-30.0 |
1900 |
3400 |
5.50 |
300 |
4.8 |
107 |
| D60 |
60 |
0.1-15.0 |
1800 |
3200 |
2.50 |
300 |
4.7 |
107 |
| D70 |
70 |
0.5-15 |
1950 |
2850 |
4.60 |
250 |
5.0 |
107 |
| D1 |
100 |
0.5-20 |
1800 |
3000 |
0.20 |
330 |
5.0 |
107 |
| D25 |
250 |
0.1-2.0 |
1500 |
2650 |
0.60 |
170 |
5.0 |
107 |
| D3 |
300 |
0.1-2.0 |
1600 |
2700 |
0.50 |
150 |
4.9 |
107 |
| D30 |
300 |
0.4-2.0 |
600 |
2600 |
0.14 |
150 |
10.0 |
107 |
| D35 |
350 |
0.1-1.5 |
1650 |
4050 |
0.50 |
170 |
5.0 |
107 |
| D38 |
380 |
0.7-0.1 |
2007 |
3375 |
0.39 |
186 |
5.11 |
107 |
| F5B |
700 |
0.1-1.5 |
1000 |
2600 |
0.48 |
130 |
5.0 |
107 |
| D8 |
800 |
0.01-0.6 |
1500 |
2900 |
0.24 |
150 |
5.0 |
107 |
| D85 |
850 |
0.1-2.0 |
1000 |
2800 |
0.30 |
130 |
4.8 |
107 |
| D9 |
900 |
0.01-0.7 |
1000 |
2700 |
0.30 |
110 |
4.7 |
107 |
| R1K |
1000 |
0.01-0.5 |
1000 |
2700 |
0.20 |
100 |
4.7 |
107 |
| D11 |
1100 |
0.01-0.6 |
600 |
2800 |
0.24 |
150 |
5.0 |
107 |
| D13 |
1300 |
0.1-0.7 |
700 |
2650 |
0.15 |
140 |
4.8 |
107 |
| D18 |
1800 |
0.01-0.6 |
600 |
2800 |
0.15 |
100 |
5.0 |
107 |
| D20 |
2000 |
0.001-0.4 |
1000 |
4000 |
0.20 |
100 |
4.7 |
107 |
Low frequency magnetic core antenna